Adds a decorative brilliance and white mirror shine to dull finishes. Best if used over Copper Mirror solution. An excellent base for rhodium, gold and silver plating.Use with pure nickel anode.Plate with solution at 140°F at 2-4 volts for 2-10 minutes.
SKU: 45.206