    Electrocleaner

    A quick and effective method of cleaning objects prior to plating. The cleaning process uses an electrolytic bath, similar to plating operations. The 2 lb size makes 8 gallons. The 5 lb size makes 20 gallons. Use with a stainless steel anode. Clean with solution heated from 120°F to 160°F at 2-6 volts for 15-30 seconds.