Produces a bright copper finish.Air bubble agitation produces superior uniformity and shine. Use with a pure copper anode. Plate with solution at room temperature at 2-3 volts for 2-10 minutes. Electroform at 1-1.3 volts for 30 minutes to 5 hours.
Clean Earth Plating Solutions (Cyanide Free)